QUESTION IMAGE
Question
identify the following weld defect.
whiskers
porosity
cold start
undercut
cracking
Analyze the visual evidence
The provided image displays a close-up photograph of a weld bead with a distinct, continuous longitudinal groove or depression running along the toe of the weld where the weld face meets the base metal. This groove represents a reduction in the cross-sectional thickness of the base metal.
Identify the defect type
Using the Welding Defects knowledge point, we evaluate the options:
- Whiskers: Unmelted electrode wire protruding through the root of the weld.
- Porosity: Gas pockets or cavities trapped within the weld metal.
- Cold start: Lack of fusion at the beginning of the weld run due to insufficient heat.
- Undercut: A groove melted into the base metal adjacent to the weld toe or weld root and left unfilled by weld metal.
- Cracking: Fracture-type interruptions within the weld or base metal.
The visual evidence of a groove melted into the base metal along the edge of the weld bead corresponds directly to the definition of an undercut.
Snap & solve any problem in the app
Get step-by-step solutions on Sovi AI
Photo-based solutions with guided steps
Explore more problems and detailed explanations
- Whiskers
- Porosity
- Cold start
- Undercut (Correct answer)
- Cracking