QUESTION IMAGE
Question
quiz
question 3 of 6
this weld defect is an example of:
burn-through
porosity
lack of penetration
excessive spatter
Analyze the visual evidence
Using the Welding Defects knowledge point
The image displays a weld bead covered with numerous small, rounded cavities, holes, or pockets scattered across and within the weld metal surface.
Identify the specific defect
Using the Porosity knowledge point
These pocket-like cavities are gas pockets trapped in the solidifying weld pool, which is the classic visual presentation of porosity.
Evaluate the other options
Using the Welding Defects knowledge point
- Burn-through is a hole completely melted through the base metal.
- Lack of penetration is a failure of the weld metal to fuse the root of the joint.
- Excessive spatter consists of small metal droplets scattered around the weld bead.
Thus, the correct option is Porosity.
Snap & solve any problem in the app
Get step-by-step solutions on Sovi AI
Photo-based solutions with guided steps
Explore more problems and detailed explanations
- Burn-through
- Porosity (Correct answer)
- Lack of penetration
- Excessive spatter